山東瀚邦膠帶有限公司的煤礦井下用MT668阻燃鋼絲繩芯輸送帶
Combustion - Resistant Steel Cord Conveyor Belt for Coal Mining
結(jié)構(gòu)
抗拉體選用高強(qiáng)度、低延伸鍍鋅鋼絲繩,上下復(fù)合配以阻燃、抗靜電優(yōu)質(zhì)覆蓋膠料,在恒張力下,通過壓合成型,硫化后,使其能適應(yīng)煤礦阻燃、導(dǎo)靜電環(huán)境下物料輸送。
Configuration
The combustion-resistant steel cord conveyor belt for coal mining is using the higher strength,less elongation galvanized steel cord.which top and bottom
surface are covered with combustion—resistant & anti—static rubber. The configuration is molded in invariable
tensile. It can convey materials in conbustion—resistant
and anti—static environments after being vulcanized
用途
適用于煤礦井下阻燃抗靜電環(huán)境下使用。具有阻燃、抗靜電,拉伸強(qiáng)度大,壽命長,使用
伸長小,成槽性好,耐曲撓性好,適用于長距離,大跨度,大運(yùn)量和高速度物料輸送。
Application
The belt has excellent perbance such as fire-resistance anti-static perbance,high strength,longevity,less elongation,good flexibility and
th roughability. It is suitable for conveying materials at the occasion of long distance, high span,large load,and high strength in fire-resistance antistatic environments.
規(guī)格型號
強(qiáng)度規(guī)格:630N/mm~4000N/mm
寬度規(guī)格:800mm~2000mm
Specification
Intensity:630N/mm~4000N/mm
Width:800mm-2000mm
主要技術(shù)指標(biāo)(MT668-1997)/Main Specification
1、覆蓋膠性能/Cover Rubber Perbance
2、鋼絲繩的粘合強(qiáng)度/Adhesion strength of steel cord
3、安全性能
(1)滾筒摩擦試驗(yàn)
每塊試樣經(jīng)滾筒摩擦試驗(yàn)時(shí), 其任何部位不得發(fā)生有焰燃燒和無焰燃燒現(xiàn)象,滾筒表面溫度不得大于325~C。
(2)酒精噴燈試驗(yàn)
對6塊具有完整覆蓋層試樣,在移去噴燈后,所有試樣的有焰燃燒時(shí)間的算術(shù)平均值和無焰燃燒時(shí)間的算術(shù)平均值不得大于3S, 其中每塊試樣的有焰燃燒時(shí)間和無焰燃燒時(shí)間單值不得大于10s。對6塊剝?nèi)ジ采w層試樣.在移去-噴燈后,所有試樣的有焰燃燒時(shí)間的算術(shù)平均值和無焰燃燒時(shí)間的算術(shù)平均值不得大于5s,其中每塊試樣的有焰燃燒時(shí)間和無焰燃燒時(shí)間單值不得大于15s。
(3)巷道丙烷燃燒試驗(yàn)
全寬度上保留的未損壞長度應(yīng)大于250mm
(4)表面電阻值
試樣上、下兩個表面的表面電阻算術(shù)平均值不得大于3*10(8次方)歐姆
產(chǎn)品介紹
3. Safety Character
(1). Drum friction test
During drum friction test, any part of test sample shall not show any sign of flame or glow The surface temperature of drum shall be less than 325℃.
(2) Combustion test with ethanol blowtorch
Average buming time with/without flame for six test samples with full covering shall be not more than 3s after ethanol bumer moving away. Each individual sample's burning time with/without flame shall be not more than 10s in the same condition.
Average buming time with/without flame for six test samples with full covering shall be not more than 5s after ethanol bumer moving away. Each individual sample's burning time with/without flame shall be not more than 15s in the same condition
(3) Laneway Propane buming test
Length that is compleby undamaged by flame shall be more than 250mm
(4) Sufface electrical resistance
Average electrical resistance of both surfaces shall be not more than 3×10(8次方)歐姆.